Minimization of Shrinkage Defect in Crankshaft Casting

Show simple item record

dc.contributor.author Abubakar, Zayyad
dc.contributor.author Ullah, Najeeb
dc.date.accessioned 2021-10-07T05:12:24Z
dc.date.available 2021-10-07T05:12:24Z
dc.date.issued 2017-11-15
dc.identifier.citation [1] Yeh-Liang Hsu, Chia-Chieh Yu, Computer Simulation Of Casting Process Of Aluminium Wheels – A Case Study, J. Engineering Manufacture, 2006, Vol. 220, Part B, 203-211 [2] S. Ji, K. Reberts, Z.Fan. Scr Mater. 2006; 55: 971-974 [3] S. Kuyucak, “Sponsored Research: Clean Steel Casting production – Evaluation of Laboratory Castings”, American Foundry Society, 2007 [4]. J.S. Campbell, “Principles of Manufacturing Materials and Processes”, Tata McGraw Hill Book Co. Inc., New Delhi,1992D.C. Ekey & W.P. Winter, “Introduction to Foundry Technology”, McGraw Hill Book Co. Inc., New York, 1958 [5] Wilson, P.E., Dell, L. D., & Anderson, G. F., (1993), “Root Cause Analysis: A Tool for Total Quality Management”, Milwaukee: ASQC Quality Press, pp-111-120 [6] (Ogura, 1995) [7] (Ying & Tao, 2011) [8] (Lee & Gokhale, 2006) [9] You, I. C., Chu, C. N. and Kashyap, R. L. 1994. “Expert Systems for Casting Design Evaluation”. In Handbook of Expert Systems, Applications in Manufacturing, Chapman & Hall Publications [10] Int. J. Mech. Eng. & Rob. Res. 2012 [11] International Journal of Research in Advent Technology, Vol.2, No.3, March 2014 E-ISSN: 2321-9637 en_US
dc.identifier.uri http://hdl.handle.net/123456789/1116
dc.description Supervised by Mr. Shariful Islam Chowdhury, Department of Mechanical and Chemical Engineering (MCE), Islamic University of Technology (IUT), Board Bazar, Gazipur-1704, Bangladesh. en_US
dc.description.abstract In our present study, we mainly focused on the reduction of the casting and moulding defects that mainly occurs during metallurgical process and we are able to depict some of those severe problems that might hamper the casting procedure. Among them temperature gradient, time difference in alloy solidification, surface area of casting material, impact of varied amount of volume of molten metal and the shape of the mould opening which we concluded should be squared instead of tapered to enhance the performance of the casting process. en_US
dc.language.iso en en_US
dc.publisher Department of Mechanical and Production Engineering (MPE),Islamic University of Technology(IUT), Board Bazar, Gazipur, Bangladesh en_US
dc.title Minimization of Shrinkage Defect in Crankshaft Casting en_US